Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 89.3 J | 65.9 ft-lb | ASTM D3763 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Dart Drop, Total Energy | 89.3 J | 65.9 ft-lb | 3.39 m/sec; ASTM D3763 |
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip.. |