Polymer Property : Dart Drop, Total Energy = 69.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific)
Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex..
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Asia Pacific)
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX1619 PC
Lexan* LUX1619 Polycarbonate resin is an extrusion grade. It is UL94 HB rated. It was designed for high light reflectance.
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX2289 PC
Lexan* LUX2289 resin is an injection molding grade with high light reflectance
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East)
Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX2619 PC
Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance.
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East)
Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance.
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML7647 PC (Asia Pacific)
Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML7647K PC (Asia Pacific)
Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific)
Low odor grade for IC tray application