Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 101 PC (Asia Pacific) Nonhalogenated, 7.0 MFR, for thicker sections without sinks. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 101R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 104R PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant in limited colors.Effective January 15.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 121R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 131R PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 153R PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 193 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 194 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 221 PC 17.5 MFR, for small, intricate parts. Improved flame retardance.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 223R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® LS2 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® LS2 PC (Asia Pacific) Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® OQ4320R PC Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® OQ4320R PC (Asia Pacific) Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® RL7517 PC FDA compliant (color limited). 2.5 MFR. Potable water/extrusion blowmolding applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 143R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific) Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 940A PC Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 940A PC (Asia Pacific) Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |