Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 510 MPa @# of Cycles 2.00e+6 |
74000 psi @# of Cycles 2.00e+6 |
R=smin/smax=0.1;RT; 50% probability of failure |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Fatigue Strength | 510 MPa | 74000 psi | Endurance Limit (Unnotched) |
Meehanite K-405 Austempered Ductile Iron Type K-405 is for applications involving wear and requiring high tensile and endurance limit. Excellent founding properties enable more accurate castings with savings in machine stock required. Da.. |