Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 4.00 MPa @# of Cycles 1.00e+6 |
580 psi @# of Cycles 1.00e+6 |
1 Hz |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |