Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 295 MPa @# of Cycles 1.00e+8 |
42800 psi @# of Cycles 1.00e+8 |
rotating beam |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ.. |