Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 290 MPa @# of Cycles 1.00e+8 |
42000 psi @# of Cycles 1.00e+8 |
rotating beam |
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Fatigue Strength | 290 MPa @# of Cycles 1.00e+7 |
42000 psi @# of Cycles 1.00e+7 |
Unnotched |
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |