Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 767 MPa | 111000 psi | R=smin/smax=0.1; 2 million cycles, F50 |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |