Polymer Property : Fatigue Strength = 310 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 310 - 360 MPa

@# of Cycles 1.00e+8
45000 - 52200 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R..
Fatigue Strength 310 - 340 MPa

@# of Cycles 1.00e+8
45000 - 49300 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 25 Strip; HT (TH04) Temper (UNS C17200)
Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 74%Superficial Hardness: 30N 58-6..
Fatigue Strength >= 310 MPa

@# of Cycles 1.00e+7
>= 45000 psi

@# of Cycles 1.00e+7
(R=-1)
Schmolz + Bickenbach MoldMAX HH® High Hard - Copper Alloy
Description: Brush Wellman’s MoldMAX HH® (High Hard) is the premier copper mold alloy. This alloy has a hardness and strength comparable with standard tool steels but its thermal conductivit..
Fatigue Strength >= 310 MPa

@# of Cycles 1.00e+7
>= 45000 psi

@# of Cycles 1.00e+7
(R=-1)
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy
Description: Brush Wellman’s MoldMAX LH® (Low Hard) is a premium copper mold alloy that provides hardness and strength comparable with standard AISI P-20 tool steel and a thermal conductivit..