Mechanical Properties Metric English Comments
Peel Strength 6.84 kN/m

@Temperature 91.0 °C
39.0 pli

@Temperature 196 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Peel Strength 6.84 kN/m

@Temperature 60.0 °C,
Time 605000 sec
39.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF/SW, Graphite/BMI
3M AC-350 Class C-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 6.84 kN/m

@Temperature 60.0 °C,
Time 605000 sec
39.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF/SW, Graphite/BMI
3M AC-350 Class C-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 6.84 kN/m

@Temperature 60.0 °C,
Time 605000 sec
39.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF/SW, Graphite/BMI
3M AC-350 Class C-8(24) Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 6.84 kN/m

@Temperature 82.0 °C
39.0 pli

@Temperature 180 °F
Aluminum Bell Pell; ASTM D3167
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..