Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.80 kN/m @Temperature 85.0 °C |
16.0 pli @Temperature 185 °F |
resistance to glass; ASTM D3167 |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Peel Strength | 2.80 kN/m @Temperature 21.1 °C |
16.0 pli @Temperature 70.0 °F |
Bell Peel |
Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 .. |
|||
Peel Strength | 2.80 kN/m @Time 259000 sec |
16.0 pli @Time 72.0 hour |
Adhesion to Glass; ASTM D3330 |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.80 kN/m @Temperature 24.0 °C, Time 86400 sec |
16.0 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Peel Strength | 2.80 kN/m @Temperature 24.0 °C, Time 86400 sec |
16.0 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Peel Strength | 2.80 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
16.0 pli @Temperature 151 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 2.80 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
16.0 pli @Temperature 151 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 2.80 kN/m @Temperature 23.0 °C |
16.0 pli @Temperature 73.4 °F |
180° T-Peel, Neoprene/CRS |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 2.80 kN/m @Time 259000 sec |
16.0 pli @Time 72.0 hour |
Adhesion to Acrylic; ASTM D3330 |
3M 4411B Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.80 kN/m @Time 259000 sec |
16.0 pli @Time 72.0 hour |
Adhesion to PP; ASTM D3330 |
3M 4411B Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.80 kN/m @Time 259000 sec |
16.0 pli @Time 72.0 hour |
Adhesion to Stainless; ASTM D3330 |
3M 4411G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.80 kN/m @Time 259000 sec |
16.0 pli @Time 72.0 hour |
Adhesion to ABS; ASTM D3330 |
3M 4411G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.80 kN/m @Time 259000 sec |
16.0 pli @Time 72.0 hour |
Adhesion to PC; ASTM D3330 |
3M 4411N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.80 kN/m @Time 259000 sec |
16.0 pli @Time 72.0 hour |
Adhesion to ABS; ASTM D3330 |
3M 4411N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.80 kN/m @Time 259000 sec |
16.0 pli @Time 72.0 hour |
Adhesion to PVC; ASTM D3330 |
3M 4411N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.80 kN/m @Temperature 49.0 °C, Time 86400 sec |
16.0 pli @Temperature 120 °F, Time 24.0 hour |
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, VMP |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |
|||
Peel Strength | 2.80 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
16.0 pli @Temperature 151 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |