Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.526 kN/m @Temperature -55.0 °C |
3.00 pli @Temperature -67.0 °F |
180° |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Peel Strength | 0.526 - 0.877 kN/m @Temperature -55.0 °C |
3.00 - 5.00 pli @Temperature -67.0 °F |
Aluminum, T-Peel |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Peel Strength | 0.526 kN/m @Temperature 23.0 °C |
3.00 pli @Temperature 73.4 °F |
180° T-Peel, Black SBR/CRS |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 0.526 kN/m @Temperature 175 °C |
3.00 pli @Temperature 347 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.526 kN/m @Temperature 175 °C |
3.00 pli @Temperature 347 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.526 kN/m @Temperature 175 °C |
3.00 pli @Temperature 347 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.526 kN/m @Temperature 175 °C |
3.00 pli @Temperature 347 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.526 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
3.00 pli @Temperature 180 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |
|||
Peel Strength | 0.526 kN/m @Temperature 49.0 °C |
3.00 pli @Temperature 120 °F |
180° |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
Peel Strength | 0.526 kN/m @Temperature -55.0 °C |
3.00 pli @Temperature -67.0 °F |
180° |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |