Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 415 MPa @Thickness 7.90 - 25.0 mm |
60200 psi @Thickness 0.311 - 0.984 in |
Typical Strength; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Tensile Strength | 415 MPa @Thickness 25.0 - 60.0 mm |
60200 psi @Thickness 0.984 - 2.36 in |
Typical Strength; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Tensile Strength | 415 MPa @Thickness 60.0 - 155 mm |
60200 psi @Thickness 2.36 - 6.10 in |
Typical Strength; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Tensile Strength | >= 415 MPa @Thickness 38.1 - 76.2 mm |
>= 60200 psi @Thickness 1.50 - 3.00 in |
Tempers T651 / T652 |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength | >= 415 MPa @Thickness 76.2 - 127 mm |
>= 60200 psi @Thickness 3.00 - 5.00 in |
Tempers T651 / T652 |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength | 415 MPa @Thickness 35.0 - 60.0 mm |
60200 psi @Thickness 1.38 - 2.36 in |
Typical Strength |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |