Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 144 MPa @Temperature 150 °C |
20900 psi @Temperature 302 °F |
ASTM D638 |
DuPont Performance Polymers VESPEL TP-8474 Polyimide DuPont Vespel TP-8474 parts are specified for mechanical, thermal, and tribological properties. TP-8474 parts offer excellent strength and toughness, dimensional stability, low outgassing, radiation.. |