DuPont Performance Polymers VESPEL TP-8474 Polyimide

Category Polymer , Thermoplastic , Polyimide, Thermoplastic
Manufacturer DuPont Performance Polymers
Trade Name VESPEL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers VESPEL TP-8474 Polyimide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DuPont Vespel TP-8474 parts are specified for mechanical, thermal, and tribological properties. TP-8474 parts offer excellent strength and toughness, dimensional stability, low outgassing, radiation resistance, creep resistance, and low coefficient of theInformation provided by DuPont Performance Polymers
Mechanical Properties Metric English Comments
Tensile Strength 144 MPa

@Temperature 150 °C
20900 psi

@Temperature 302 °F
ASTM D638
229 MPa

@Temperature 23.0 °C
33200 psi

@Temperature 73.4 °F
ASTM D638
Flexural Modulus 17.2 GPa

@Temperature 23.0 °C
2490 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Temperature 23.0 °C
2.06 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 228
CTE, linear, Transverse to Flow 6.00 µm/m-°C

@Temperature 23.0 - 150 °C
3.33 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 228
Descriptive Properties Value Comments
Appearance Natural Color
Forms Shapes
Material Status Current
Region Available - Global Yes
RoHS Compliance Contact Manufacturer