Mechanical Properties Metric English Comments
Tensile Strength >= 540 MPa

@Thickness 9.90 - 12.5 mm
>= 78300 psi

@Thickness 0.390 - 0.492 in
Temper T651; Standard EN 485-2
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength >= 540 MPa

@Thickness 12.5 - 25.0 mm
>= 78300 psi

@Thickness 0.492 - 0.984 in
Temper T651; Standard EN 485-2
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength 540 MPa

@Thickness 60.0 - 80.0 mm
78300 psi

@Thickness 2.36 - 3.15 in
Typical Strength
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength >= 540 MPa

@Thickness 127 - 152.4 mm
>= 78300 psi

@Thickness 5.00 - 6.000 in
Tempers T651 / T652
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength >= 540 MPa

@Thickness 7.90 - 12.5 mm
>= 78300 psi

@Thickness 0.311 - 0.492 in
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Tensile Strength >= 540 MPa

@Thickness 12.5 - 25.0 mm
>= 78300 psi

@Thickness 0.492 - 0.984 in
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Tensile Strength >= 540 MPa

@Thickness 40.0 - 50.0 mm
>= 78300 psi

@Thickness 1.57 - 1.97 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Copyright © lookpolymers.com All Rights Reserved