Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 5.87 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 5.87 MPa

@Strain 100 %
851 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Elastamax™ HTE 3070 Polyvinyl Chloride + NBR (PVC+NBR)
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a..
Tensile Strength 5.87 MPa

@Strain 100 %
851 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Elastamax™ HTE 3170 Polyvinyl Chloride + NBR (PVC+NBR)
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a..