Mechanical Properties Metric English Comments
Tensile Strength 414 MPa

@Diameter 12.7 - 25.4 mm
60000 psi

@Diameter 0.500 - 1.00 in
Rod H02
Mueller Ecostreamâ„¢ C36300 Copper Zinc Lead Alloy
As one of the low lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36300 alloy provides a viable alternative to those manufacturers who are manufacturing ..
Tensile Strength >= 414 MPa

@Thickness 76.2 - 101.6 mm
>= 60000 psi

@Thickness 3.00 - 4.000 in
Tempers T851/T852)
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..