Tensile Strength 350 MPa

@Thickness 8.00 - 25.0 mm
50800 psi

@Thickness 0.315 - 0.984 in
Typical Strength; Standard EN 485-2
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength 350 MPa

@Thickness 25.0 - 60.0 mm
50800 psi

@Thickness 0.984 - 2.36 in
Typical Strength; Standard EN 485-2
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength 350 MPa

@Thickness 60.0 - 150 mm
50800 psi

@Thickness 2.36 - 5.91 in
Typical Strength; Standard EN 485-2
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength 350 MPa

@Thickness 4.99 - 20.0 mm
50800 psi

@Thickness 0.196 - 0.787 in
Typical Strength
Constellium Planoxal® 60 Aluminum plate
The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use..
Tensile Strength 350 MPa

@Thickness 20.0 - 80.0 mm
50800 psi

@Thickness 0.787 - 3.15 in
Typical Strength
Constellium Planoxal® 60 Aluminum plate
The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use..
Tensile Strength 350 MPa

@Thickness 9.90 - 25.0 mm
50800 psi

@Thickness 0.390 - 0.984 in
Typical Strength
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
Tensile Strength 350 MPa

@Thickness 25.0 - 60.0 mm
50800 psi

@Thickness 0.984 - 2.36 in
Typical Strength
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
Tensile Strength 350 MPa

@Thickness 60.0 - 140 mm
50800 psi

@Thickness 2.36 - 5.51 in
Typical Strength
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
Copyright © lookpolymers.com All Rights Reserved