Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 300 MPa @Thickness 8.00 - 25.0 mm |
43500 psi @Thickness 0.315 - 0.984 in |
Typical Strength |
Constellium DOKIMA® Rolled Plate Aluminum DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct.. |
|||
Tensile Strength | 300 MPa @Thickness 25.0 - 60.0 mm |
43500 psi @Thickness 0.984 - 2.36 in |
Typical Strength |
Constellium DOKIMA® Rolled Plate Aluminum DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct.. |
|||
Tensile Strength | 300 MPa @Thickness 60.0 - 100 mm |
43500 psi @Thickness 2.36 - 3.94 in |
Typical Strength |
Constellium DOKIMA® Rolled Plate Aluminum DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct.. |
|||
Tensile Strength | 300 MPa @Thickness 100 - 150 mm |
43500 psi @Thickness 3.94 - 5.91 in |
Typical Strength |
Constellium DOKIMA® Rolled Plate Aluminum DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct.. |
|||
Tensile Strength | >= 300 MPa @Thickness 6.00 - 12.5 mm |
>= 43500 psi @Thickness 0.236 - 0.492 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | >= 300 MPa @Thickness 6.00 - 12.0 mm |
>= 43500 psi @Thickness 0.236 - 0.472 in |
Temper T651; Standard EN 485-2 |
Constellium Planoxal® 60 Aluminum plate The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use.. |
|||
Tensile Strength | >= 300 MPa @Thickness 9.90 - 12.5 mm |
>= 43500 psi @Thickness 0.390 - 0.492 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |
|||
Tensile Strength | 300 MPa @Treatment Temp. 1000 °C |
43500 psi @Treatment Temp. 1830 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |