Mechanical Properties Metric English Comments
Tensile Strength >= 175 MPa

@Temperature 199 °C
>= 25400 psi

@Temperature 390 °F
H.C. Starck NRC® Tantalum (UNS R05200)
Applications: High strength and excellent corrosion resistance make tantalum ideal for use in the manufacture and repair of chemical process equipment and heat exchangers. Other uses are rupture di..
Tensile Strength 175 MPa

@Temperature 25.0 °C
25400 psi

@Temperature 77.0 °F
ASTM D 638
Saint-Gobain Meldin® 1003 Thermoplastic Bearing Material
Meldin 1003 components offer the highest level of strength and rigidity for this product family. They maintain high chemical, tensile, and flexural properties even at elevated temperatures.MeldinÂ..
Tensile Strength 175 MPa

@Strain 1.00 %,
Temperature 23.0 °C
25400 psi

@Strain 1.00 %,
Temperature 73.4 °F
5mm/min
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Tensile Strength 175 MPa

@Temperature 70.0 °C,
Time 720000 sec
25400 psi

@Temperature 158 °F,
Time 200 hour
62% RH
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
Tensile Strength 175 MPa

@Treatment Temp. 220 °C,
Time 5.40e+6 sec
25400 psi

@Treatment Temp. 428 °F,
Time 1500 hour
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..
Tensile Strength 175 MPa

@Treatment Temp. 220 °C,
Time 9.00e+6 sec
25400 psi

@Treatment Temp. 428 °F,
Time 2500 hour
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..