Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 10.0 MPa @Strain 2.00 %, Temperature 100 °C |
1450 psi @Strain 2.00 %, Temperature 212 °F |
50mm/min |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Tensile Strength | 10.0 MPa @Strain 1.00 %, Temperature 100 °C |
1450 psi @Strain 1.00 %, Temperature 212 °F |
ISO 527 |
BASF Ultramid® B3S HP PA6 (Dry) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |