Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00410 GPa | 0.595 ksi | Dry Modulus of Rupture, 50% clay/50% flint, cast bars |
Old Hickory FC-120 Tennessee Ball Clay The FC-120 clay is a special selection for sanitaryware. It is very fast casting and is designed to use in combination with the C-33A or other finer particle size distribution clay. The FC-120 provi.. |
|||
Modulus of Rupture | 0.00410 GPa @Temperature 816 °C |
0.595 ksi @Temperature 1500 °F |
|
Zircar Ceramics AX-200 Refractory Supported Heater ZIRCAR Refractory Supported Heater Type AX-200 consists of high temperature, helically-wound, iron-chrome-aluminum metallic alloy resistance heating elements fully embedded in a strong, highly stabl.. |
|||
Modulus of Rupture | 0.00410 GPa @Temperature 1371 °C |
0.595 ksi @Temperature 2500 °F |
ASTM C268 |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |