Mechanical Properties Metric English Comments
Modulus of Rupture 0.00280 - 0.00350 GPa

@Treatment Temp. 750 °C,
Time 86400 sec
0.406 - 0.508 ksi

@Treatment Temp. 1380 °F,
Time 24.0 hour
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications
Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant..
Modulus of Rupture 0.00280 - 0.00350 GPa

@Treatment Temp. 750 °C,
Time 86400 sec
0.406 - 0.508 ksi

@Treatment Temp. 1380 °F,
Time 24.0 hour
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications
Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol..
Modulus of Rupture 0.00280 GPa

@Temperature 104 °C
0.406 ksi

@Temperature 219 °F
Dried; ASTM C268
BNZ Materials Blazecrete 2600 Dense Castable
Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as..
Modulus of Rupture 0.00280 GPa

@Temperature 540 °C
0.406 ksi

@Temperature 1000 °F
Fired; ASTM C268
BNZ Materials Blazecrete 3000 Dense Castable
Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec..