Modulus of Rupture 0.00176 GPa
0.255 ksi
Green
Unifrax Fibermax® Duraboard® 18R Board
Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. ..