Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 22.1 GPa @Temperature 177 °C |
3210 ksi @Temperature 351 °F |
|
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel |
|||
Compressive Modulus | 22.1 GPa @Temperature 93.0 °C |
3210 ksi @Temperature 199 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric Information provided by HexCel |
|||
Compressive Modulus | 22.1 GPa @Temperature 24.0 °C |
3210 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric Information provided by HexCel |
|||
Compressive Modulus | 22.1 GPa @Temperature 71.0 °C |
3210 ksi @Temperature 160 °F |
1/2 hr |