Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 38.9 GPa @Temperature 23.0 °C |
5640 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |