Polymer Property : Compressive Modulus = 20.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 20.0 GPa

@Temperature 93.3 °C
2900 ksi

@Temperature 200 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 20.0 GPa

@Temperature 21.1 °C
2900 ksi

@Temperature 70.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 20.0 GPa

@Temperature 177 °C
2900 ksi

@Temperature 351 °F
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F161; Fiber: 450-1/2Information provided by HexCel