Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00109 GPa @Strain 20.0 % |
0.158 ksi @Strain 20.0 % |
|
Vicone High Performance Rubber VicoFluorâ„¢ C105LF-BL High Performance Fluoroelastomer Information provided by Vicone |