| Category | Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE) |
| Manufacturer | Vicone High Performance Rubber |
| Trade Name | VicoFluor™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Vicone High Performance Rubber VicoFluor™ C105LF-BL High Performance Fluoroelastomer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D3165 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 47 | 47 | ASTM D2240 |
| 51.23 <br>@Treatment Temp. 200 °C,<br> Time 252000 sec |
51.23 <br>@Treatment Temp. 392 °F,<br> Time 70.0 hour |
Heat Aging; ASTM D573 | |
| Tensile Strength, Yield | 9.00 MPa | 1310 psi | ASTM D412 |
| 8.47 MPa <br>@Treatment Temp. 200 °C,<br> Time 252000 sec |
1230 psi <br>@Treatment Temp. 392 °F,<br> Time 70.0 hour |
Heat Aging; ASTM D573 | |
| Elongation at Break | 319 % | 319 % | ASTM D412 |
| 250 % <br>@Treatment Temp. 200 °C,<br> Time 252000 sec |
250 % <br>@Treatment Temp. 392 °F,<br> Time 70.0 hour |
Heat Aging; ASTM D573 | |
| Compressive Modulus | 0.000300 GPa <br>@Strain 5.00 % |
0.0435 ksi <br>@Strain 5.00 % |
|
| 0.000480 GPa <br>@Strain 10.0 % |
0.0696 ksi <br>@Strain 10.0 % |
||
| 0.00109 GPa <br>@Strain 20.0 % |
0.158 ksi <br>@Strain 20.0 % |
||
| 0.00158 GPa <br>@Strain 25.0 % |
0.229 ksi <br>@Strain 25.0 % |
||
| Compression Set | 6.35 % <br>@Temperature 175 °C,<br> Time 79200 sec |
6.35 % <br>@Temperature 347 °F,<br> Time 22.0 hour |
ASTM D395 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Blue |