Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 34.3 - 44.1 MPa @Temperature 1350 °C, Time 10800 sec |
4980 - 6400 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 44.1 MPa @Temperature 1500 °C, Time 10800 sec |
3560 - 6400 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TPA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |