Mechanical Properties Metric English Comments
Compressive Strength 20.0 MPa

@Strain 5 %
2900 psi

@Strain 5 %
ISO 604
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data)
This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica..
Compressive Strength 20.0 MPa

@Strain 1 %
2900 psi

@Strain 1 %
ISO 604
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data)
Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to..
Compressive Strength 20.0 MPa

@Strain 5 %
2900 psi

@Strain 5 %
ISO 604
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data)
Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 110 C Dense Refractory Castable
Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 C Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 100 °C
2900 - 4350 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 100 °C
2900 - 4350 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable
Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable
Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1400 °C
2900 - 4350 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 GM Dense Refractory Castable
Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 100 C Dense Refractory Castable
Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values ..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1300 °C
2900 - 4350 psi

@Temperature 2370 °F
Cold Crushing Strength