Compressive Strength 190 MPa

@Temperature 120 °C
27600 psi

@Temperature 248 °F
ISO 604
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
Compressive Strength 190 - 210 MPa

@Temperature 1400 °C
27600 - 30500 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 160 H SiC (R) Dense Self Flowing Refractory Castable
Description: Flucon 160 H SiC (R) is a self-flowing low cement castable, characterized by a high strength and good slag resistance. Because of the presence of SiC this material has a very good resis..
Compressive Strength 190 MPa

@Strain 5 %
27600 psi

@Strain 5 %
ISO 604
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data)
This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s..
Compressive Strength 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..