Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 188 MPa @Temperature 23.0 °C |
27300 psi @Temperature 73.4 °F |
JIS K7208 |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Compressive Strength | 188 MPa @Temperature 22.8 °C |
27300 psi @Temperature 73.0 °F |
JIS K7208 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |