Compressive Strength 0.159 MPa

@Temperature 21.1 °C
23.0 psi

@Temperature 70.0 °F
Dry; ASTM D695
Renegade Materials Corporation RM-3006 Bismaleimide (BMI) Paste Adhesive
Developed using state-of-the-art formulating technologies, RM-3006 BMI Paste Adhesive is a -65°F to 400°F (-54°C to 204°C) service material. RM-3006 was developed for use with Renegade’s BMI P..