Polymer Property : Compressive Strength = 1740 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 12.0 MPa

@Strain 1 %
1740 psi

@Strain 1 %
ISO 604
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
Compressive Strength 12.0 MPa

@Strain 1 %
1740 psi

@Strain 1 %
ISO 604
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data)
This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to..
Compressive Strength 12.0 MPa

@Strain 2 %
1740 psi

@Strain 2 %
ISO 604
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data)
TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance
Compressive Strength 12.0 - 18.0 MPa

@Temperature 100 °C
1740 - 2610 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable
Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information..
Compressive Strength 12.0 - 18.0 MPa

@Temperature 1600 °C
1740 - 2610 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast CURON 185 T Dense Refractory Castable
Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values ..
Compressive Strength 12.0 - 18.0 MPa

@Temperature 100 °C
1740 - 2610 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable
Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere...