Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 95.0 MPa @Temperature 200 °C |
13800 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Compressive Strength | 95.0 MPa @Temperature 200 °C |
13800 psi @Temperature 392 °F |
ISO 604 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Compressive Strength | 95.0 - 105 MPa @Temperature 1000 °C |
13800 - 15200 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar.. |
|||
Compressive Strength | 95.0 - 105 MPa @Temperature 1300 °C |
13800 - 15200 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack.. |
|||
Compressive Strength | 95.0 - 105 MPa @Temperature 1400 °C |
13800 - 15200 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 H SiC Dense Vibrating Refractory Castable Description: Vibron 160 H SiC is a low cement vibrating castable characterized by a high strength, good abrasion resistance and excellent thermal shock resistance. Because of the presence of SiC, th.. |