Mechanical Properties Metric English Comments
Compressive Strength 85.0 MPa

@Strain 5 %
12300 psi

@Strain 5 %
ISO 604
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data)
Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette..
Compressive Strength 85.0 MPa

@Strain 5 %
12300 psi

@Strain 5 %
ISO 604
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data)
This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie..
Compressive Strength 85.0 MPa

@Strain 5 %
12300 psi

@Strain 5 %
ISO 604
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data)
Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr..
Compressive Strength 85.0 - 95.0 MPa

@Temperature 100 °C
12300 - 13800 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material
Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i..
Compressive Strength 85.0 - 95.0 MPa

@Temperature 100 °C
12300 - 13800 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material
Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T..
Compressive Strength 85.0 - 95.0 MPa

@Temperature 1300 °C
12300 - 13800 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable
Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc..
Compressive Strength 85.0 - 95.0 MPa

@Temperature 100 °C
12300 - 13800 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 150 G Dense Vibrating Refractory Castable
Description: Vibron 150 G is a low cement castable based on sintered South-American bauxite. Especially suited for direct contact with liquid aluminum metal.Remarks: Indicated values apply to vibrat..
Compressive Strength 85.0 - 95.0 MPa

@Temperature 100 °C
12300 - 13800 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 180 T Dense Vibrating Refractory Castable
Description: Vibron 180 T is a low cement castable, based on tabular alumina.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.