Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 70.0 MPa @Temperature 120 °C |
10200 psi @Temperature 248 °F |
Result based on 450G; ISO 604 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Compressive Strength | 70.0 MPa @Temperature 200 °C |
10200 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Compressive Strength | 70.0 MPa @Temperature 200 °C |
10200 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Compressive Strength | 70.0 MPa @Temperature 120 °C |
10200 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Compressive Strength | 70.0 MPa @Temperature 200 °C |
10200 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Compressive Strength | 70.0 - 90.0 MPa @Temperature 100 °C |
10200 - 13100 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p.. |
|||
Compressive Strength | 70.0 MPa @Temperature 120 °C |
10200 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |