Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 7.85 MPa @Temperature 800 °C |
1140 psi @Temperature 1470 °F |
Cold Crushing |
Sharadaa Ceramics Sharada LTM 1.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 7.85 MPa @Temperature 110 °C, Time 86400 sec |
1140 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories APC-120G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 7.85 MPa @Temperature 110 °C, Time 86400 sec |
1140 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories TD-R75 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |