Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 66.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 66.7 MPa

@Temperature 1000 °C,
Time 10800 sec
9670 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 66.7 MPa

@Temperature 1000 °C,
Time 10800 sec
9670 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-85AL Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved