Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 61.0 MPa @Strain 2 % |
8850 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data) Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal fo.. |
|||
Compressive Strength | 61.0 MPa @Strain 2 % |
8850 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Compressive Strength | 61.0 MPa @Strain 2 % |
8850 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data) This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear.. |