Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 30.4 MPa @Temperature 1450 °C, Time 7200 sec |
4410 psi @Temperature 2640 °F, Time 2.00 hour |
Cold Crushing Strength |
Chosun Refractories AU3 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |