Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 3.50 - 4.50 MPa @Temperature 100 °C |
508 - 653 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re.. |
|||
Compressive Strength | 3.50 - 4.50 MPa @Temperature 100 °C |
508 - 653 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE LW Refractory Insulating Castable Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also ava.. |
|||
Compressive Strength | 3.50 - 4.50 MPa @Temperature 100 °C |
508 - 653 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod.. |
|||
Compressive Strength | 3.50 - 4.50 MPa @Temperature 1200 °C |
508 - 653 psi @Temperature 2190 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod.. |