Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Compressive Strength | 210 MPa @Temperature 120 °C |
30500 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Compressive Strength | 210 MPa @Temperature 120 °C |
30500 psi @Temperature 248 °F |
ISO 604 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |