Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 17.5 MPa @Strain 5 % |
2540 psi @Strain 5 % |
ISO 604 |
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data) By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey.. |
|||
Compressive Strength | 17.5 MPa @Strain 5 % |
2540 psi @Strain 5 % |
ISO 604 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Compressive Strength | 17.5 MPa @Strain 5 % |
2540 psi @Strain 5 % |
ISO 604 |
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data) This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b.. |
|||
Compressive Strength | 17.5 MPa @Temperature 110 °C, Time 86400 sec |
2530 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories RSP-M Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |