Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 12.0 MPa @Strain 1 % |
1740 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Compressive Strength | 12.0 MPa @Strain 1 % |
1740 psi @Strain 1 % |
ISO 604 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Compressive Strength | 12.0 MPa @Strain 2 % |
1740 psi @Strain 2 % |
ISO 604 |
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data) TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance |
|||
Compressive Strength | 12.0 - 18.0 MPa @Temperature 100 °C |
1740 - 2610 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information.. |
|||
Compressive Strength | 12.0 - 18.0 MPa @Temperature 1600 °C |
1740 - 2610 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 185 T Dense Refractory Castable Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values .. |
|||
Compressive Strength | 12.0 - 18.0 MPa @Temperature 100 °C |
1740 - 2610 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere... |