Mechanical Properties Metric English Comments
Compressive Strength 10.5 MPa

@Strain 1 %
1520 psi

@Strain 1 %
ISO 604
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data)
This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica..
Compressive Strength 10.5 MPa

@Strain 2 %
1520 psi

@Strain 2 %
ISO 604
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data)
TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C.
Compressive Strength 10.5 MPa

@Strain 2 %
1520 psi

@Strain 2 %
ISO 604
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data)
TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an..
Compressive Strength 10.5 MPa

@Strain 5 %
1520 psi

@Strain 5 %
ISO 604
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data)
TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid..
Compressive Strength 10.5 MPa

@Strain 2 %
1520 psi

@Strain 2 %
ISO 604
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data)
This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000.
Compressive Strength 10.5 MPa

@Strain 1 %
1520 psi

@Strain 1 %
ISO 604
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data)
Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg..
Compressive Strength 10.5 MPa

@Temperature 110 °C,
Time 86400 sec
1520 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories CO-210 Blast Furnace Runner Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved