Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 120 °C |
392 ksi @Temperature 248 °F |
|
LATI Lapex A PES Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 60.0 °C |
392 ksi @Temperature 140 °F |
|
LATI Lapex R PPSU Polyphenylene Sulfone (PPSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 120 °C |
392 ksi @Temperature 248 °F |
|
LATI Latamid 12 H2 G/30 PA 12, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
|
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
|
LATI Latan 23UV POM Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Tensile Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
|
LATI Latan 23UVE71 POM Polyoxymethylene (POM). UV stabilized. Toughened. Low viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 150 °C |
392 ksi @Temperature 302 °F |
|
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
|
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 150 °C |
392 ksi @Temperature 302 °F |
|
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail.. |