Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 55.2 MPa @Temperature 538 °C |
8000 psi @Temperature 1000 °F |
Type 316 Stainless Steel sleeve joint |
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi.. |
|||
Tensile Strength, Ultimate | 55.2 MPa @Temperature 482 °C |
8000 psi @Temperature 900 °F |
Inconel butt joint |
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet.. |